Improved Irreversibility Behaviour and Critical Current Density in MgB2-Diamond Nanocomposites
arXiv:cond-mat/0302365 · doi:10.1063/1.1606884
Abstract
MgB2-diamond nanocomposite superconductors have been synthesized by addition of nano-diamond powder. Microstructural analysis shows that the nanocomposite superconductor consists of tightly-packed MgB2 nano-grains (~50-100 nm) with highly-dispersed and uniformly-distributed diamond nanoparticles (~10-20 nm) inside the grains. The Jc-H and Hiir-T characteristics have been significantly improved in this MgB2-diamond nanocomposite, compared to MgB2 bulk materials prepared by other techniques. Also, the Jc value of 1x104 A/cm2 at 20 K and 4 T and the Hirr value of 6.4 T at 20 K have been achieved
9 pages, 5 figures