Thickness and temperature dependence of the magnetodynamic damping of pulsed laser deposited $\text{La}_{0.7}\text{Sr}_{0.3}\text{MnO}_3$ on (111)-oriented SrTi$\text{O}_3$

arXiv:1605.08195 · doi:10.1016/j.jmmm.2016.07.028

Abstract

We have investigated the magnetodynamic properties of $\text{La}_{0.7}\text{Sr}_{0.3}\text{MnO}_3$ (LSMO) films of thickness 10, 15 and 30 nm grown on (111)-oriented SrTi$\text{O}_3$ (STO) substrates by pulsed laser deposition. Ferromagnetic resonance (FMR) experiments were performed in the temperature range 100--300 K, and the magnetodynamic damping parameter $α$ was extracted as a function of both film thickness and temperature. We found that the damping is lowest for the intermediate film thickness of 15 nm with $α\approx 2 \cdot 10^{-3}$, where $α$ is relatively constant as a function of temperature well below the Curie temperature of the respective films.

Accepted for publication in Journal of Magnetism and Magnetic Materials